Product Details:
Wire Material | Ni, Cr, Ti, Al, W, Mo, Cu, Fe, etc |
Color | Silver, Black |
Types Of Thermal Spraying | Wire arc Spraying |
Dimensions | Standard sizes are 1.20, 1.60 and 2.00 mm (0.0472, 0.0693 and 0.0787 inch). Other sizes can be offer |
Usage/Application | Thermal spray wire is specially used in wire arc spraying bonding layer. |
Finish | Bright Annealed |
Bond Strength | 40-75 MPa |
Origin | German, Sweden |
Thermal spraying wire is used in a variety of applications, such as:
Material | Main components | Features | Application | |
HCF-50 | Ni, Cr, Ti | Bond strength≥48Mpa Hardness≥HRC46 Best performance of high temperature corrosion and oxidation resistance |
Boiler water wall, anti corrosion and oxidation of the superheater, turbine blade, heat and corrosion resistance in steel mill. | |
HCF-95 | Ni, Al, Ti | Bond strength≥75Mpa Strong oxidation resistance and corrosion resistance |
High temperature base material | |
HCF-25 | Ni, Cr, W, Mo | Bond strength≥45Mpa Hardness≥HRC33 Best performance of oxidation and corrosion resistance |
Wear proof of four tubes in boiler, and resistance to wear and corrosion of shaft, pump, roller, dryer, etc. | |
HCF-40 NiCrTiFe | Ni, Cr, W, Mo | Bond strength≥47Mpa Hardness≥HRC43 High performance of high temperature oxidation and corrosion resistance |
Anti oxidation and corrosion in pressure vessel. | |
HCF-80 CL-NiCr | Ni, Cr | Bond strength≥40Mpa Hardness≥HRC35 Good corrosion resistance |
Anti-corrosion in water cooled wall, superheater and reheater | |
HCF-01 | W, Al, Fe | Bond strength≥40Mpa Hardness≥HRC35 Certain performance of oxidation and corrosion resistance |
Corrosion and oxidation resistance under lower temperature | |
Monel | Ni, Cu | Resistance to hydrogen sulfide, sulfuric acid and hydrochloric acid | It is used in various containers of anti hydrogen sulfide and acid, and the repair of wear-proof parts. |